Page 388 - Construction Waterproofing Handbook
P. 388

8.48   CHAPTER EIGHT























































                            FIGURE 8.53 Damage done to substrate envelope components by insufficient EIFS
                            application. (Posted at www.new-hanover.nc.us\ins\)


                      undersized and failure has occurred due to movement exceeding the capability of
                      the sealant.
                         In other transition details where removing the existing sealant might damage the enve-
                      lope further, overbanding can be used as a remedial treatment. Figure 8.57 details the use
                      of overbanding at a window perimeter. Similar repairs can be made at protrusions and pen-
                      etrations if appropriate.