3+ 3
Neodymium (Nd , 4f )— continued
Host Laser Wavelength Temp. Optical
crystal transition ( m) (K) pump Mode Ref.
1.0837 130 Xe lamp p 439
1.0843 300 Xe lamp p 363, 439
4
YVO 4 4 F 3/2 fi I 11/2 1.0625 300 Xe lamp p 620
4
YVO 4 4 F 3/2 fi I 11/2 1.0634 300 Ar laser cw 778
1.064 300 laser diode cw 684
1.0641 300 Xe lamp p 620
1.0648 300 Xe lamp p 620
1.0664–1.0672 300–690 Xe lamp p 626, 628
1.069 ~90 Xe lamp p 987
4 F 3/2 fi I 13/2 1.34 300 Ar laser cw 778
4
4
YVO 4 4 F 3/2 fi I 13/2 1.3415 77 Xe lamp p 537
1.3425 300 Xe lamp p 537
4
ZrO -Y O 3 4 F 3/2 fi I 11/2 1.0608 300 Xe lamp p 563
2
2
4
4 F 3/2 fi I 13/2 1.3320 300 Xe lamp p 564
3+ 5
Samarium (Sm , 4f )
Host Laser Wavelength Temp. Optical
crystal transition ( m) (K) pump Mode Ref.
6
TbF 3 4 G 5/2 fi H 7/2 0.5932 116 Xe lamp p 48
3+ 6
Europium (Eu , 4f )
Host Laser Wavelength Temp. Optical
crystal transition ( m) (K) pump Mode Ref.
7
Y O 3 5 D 0 fi F 2 0.6113 220 Xe lamp p 58
2
7
YVO 4 5 D fi F 2 0.6193 90 Xe lamp p 66
0
3+ 8
Terbium (Tb , 4f )
Host Laser Wavelength Temp. Optical
crystal transition ( m) (K) pump Mode Ref.
7
LiYF :Gd 5 D fi F 5 0.5445 300 Xe lamp p 35
4