Page 118 - Handbook of Properties of Textile and Technical Fibres
P. 118
Properties of wool 99
McPhee JR: Shrinkproofing of wool with neutral permanganate or acid bromate in concentrated
sodium chloride solution, Text Res J 30:358e365, 1960b. https://doi.org/10.1177/
004051756003000504.
Millington K: Using ultraviolet radiation to reduce pilling of knitted wool and cotton, Text Res J
68:413e421, 1998. https://doi.org/10.1177/004051759806800605.
Millington KR: Photoyellowing of wool. Part 1: factors affecting photoyellowing and experi-
mental techniques, Coloration Technol 122:169e186, 2006a.
Millington KR: Photoyellowing of wool. Part 2: photoyellowing mechanisms and methods of
prevention, Coloration Technol 122:301e316, 2006b.
Montazer M, Ramin A: Influences of proteases and trans-glutaminases on wool, Fibres Text East
Eur 18:98e102, 2010.
Montgomery DJ: Effect of stiffness and nonuniformity on vibroscopic determination of filament
cross-sectional area, J Appl Phys 24:1092e1099, 1953.
Morton WE, Hearle JWS: Physical properties of textile fibres, ed 3, Manchester, 1993, The
Textile Institute.
Motaghi Z, Eskandarnejad S, Montazer M, Ardjmand M, Moghadam MB: Mechanical slen-
derizing of coarse wool fibre and determination of its characteristics with FTIR and Raman
spectroscopy, J Text Inst 103:8e18, 2012.
Motaghi Z, Eskandarnejad S, Montazer M: The influence of the coarse wool treatment on fiber
structure and physico-mechanical parameters, J Nat Fibers 11:1e12, 2014. https://doi.org/
10.1080/15440478.2013.824850.
Nachane RP, Iyer KRK: Prediction of bundle strength from single fibre test data, Text Res J 10:
639e641, 1980.
Naylor GRS, Williams VA: Pilling of wool knitwear and some related fibre mechanical prop-
erties. In Carnaby GA, Wood EJ, Story LF, editors: WRONZ special publication, Christ-
church, 1988, Wool Research Organisation of New Zealand, (WRONZ), pp 569e578. The
application of mathematics and physics in the wool industry, vol. 6.
Nogueira ACS, Nakano AK, Joekes I: Impairment of hair mechanical properties by sun exposure
and bleaching treatments, J Cosmet Sci 55:533e537, 2004.
Okamoto M, Tanji N, Habe T, Inoue S, Tokunaga S, Tanamachi H: ToF-SIMS characterization
of the lipid layer on the hair surface. II: effect of the 18-MEA lipid layer on surface hy-
drophobicity, Surf Interf Anal 43:298e301, 2011.
Orwin DFG, Thomson RW: The electron microscopy of two types of fibre damage and its
relationship to some cell components. In Proc. 5th Int. Wool Text. Res. Conf., Aachen,
1975, pp 173e183.
Orwin DFG, Woods JL, Elliott KH: Composition of the cortex of sound and tender wools. In
Proc. 6th Int. Wool Text. Res. Conf., Pretoria, 1980, pp 193e205.
Orwin DFG, Woods JL, Gourdie RG: Cortical cell type and wool strength. In Proc. 7th Int. Wool
Text. Res. Conf., Tokyo, 1985, pp 194e203.
Parbhu AN, Bryson WG, Ratneshwar L: Disulfide bonds in the outer layer of keratin fibres
confer higher mechanical rigidity: correlative nano-indentation and elasticity measurement
with AFM, Biochemistry 38:11755e11761, 1999.
Peryman RV: The effect on wool of boiling in aqueous solutions, I e solutions at pH 1.5e9 with
and without sodium sulphate, J Soc Dyers Col 70:83e92, 1954.
Peterson AD, Gherardi SG, Doyle PT: Components of staple strength in fine and broad wool
Merino hoggets run together in a Mediterranean environment, Aust J Agric Res 49:
1181e1186, 1998.