Page 158 - Construction Waterproofing Handbook
P. 158

ABOVE-GRADE WATERPROOFING  3.47


























                             FIGURE 3.25 Crack repair detailing for deck-coating applications. (Courtesy of Carlisle
                             Corporation)




























                                FIGURE 3.26 Expansion joint detailing for deck-coating applications. (Courtesy of
                                Carlisle Corporation)

                         and they should be countersunk. The screw head is filled with a urethane sealant and trow-
                         eled flush with the plywood finish (Fig. 3.29). As these coatings are relatively thin, 60–100 mil
                         dry film, their finish mirrors the substrate they are applied over. Therefore, if plywood
                         joints are uneven or knots or chips are apparent in the plywood, they also will be apparent
                         in the deck-coating finish.