Page 793 - Corrosion Engineering Principles and Practice
P. 793
742 I n d e x I n d e x 743
Microbiology influenced corrosion National Association of Corrosion
(MIC) (Cont.): Engineers (NACE) International
plaktonic, 409–411 (Cont.):
sessile, 409–411 certification program of, 7–8
and sticky polymers, 409 CIP 1-day bridge Specialty Course, 7
and underdeposit acid attacks, 409 Corrosion Control in the Refining
Microorganisms (see Microbes) Industry, 7
Mineral constituents, in fresh water, 269 on cost of corrosion damage, 14
Mixed-acid isocorrosion diagrams, 435 CP 3—Cathodic Protection
Models and modeling: Technologist course, 7
for ICCP, 579–582 CP 4—Cathodic Protection
and interference, 582–585 Specialist, 7
for kinetic principles, 678–680 CP Tutorials, 7
Moisture curing polyurethane and Department of Transportation, 14
(MCU), 601 on economic calculations, 441
Moisture vapor transfer, 590 Internal Corrosion Technologist
Moisture-cured inorganic silicate, 607 Course, 7
Molten salts, 708 International Corrosion Network, 11
Molybdenum (molybond): Marine Coating Inspector Course, 7
for spray coat, 632 Protective Coatings and Linings, 7
temperatures affecting, 675 Successful Coating and Lining of
Monel, 378, 632 Concrete, 7
Monitoring, 121–134 on water jettings, 658–659
with CMAS, 132–134 National Roofing Contractors
with EIS, 123–124 Association (NRCA), 170
with ENA, 124–132 Natural gases, 508
field corrosion, 129 Natural waters, 268–286
risk-based inspection for, 505–506 brackish water, 277
thin film corrosion, 129 fresh water, 269–276
with zero resistance ammetry, 122–123 seawater, 277–284
Morpholine, 622 Nernst, Walther, 54
Morpholine nitrate, 622 Nernst diffusion layer, 93–94
MTI (Materials Technology Nernst equation, 54–55
Institute), 478 Neutral solutions:
Mud cracking, 591 chemical reactions in, 32–33
Multimet, 686, 692 corrosion in, 32–33
and galvanic series, 228
and sea-water, 229
N Nickel, 686
NACE (see National Association of atmospheric corrosion of, 376–377
Corrosion Engineers deposits of, 629
International) electrodeposited, 376
NACE Basic Corrosion Course, 7 for spray coat, 632
NACE CP 3—Cathodic Protection stress corrosion cracking in, 200
Technologist course, 7 temperatures affecting, 678, 706
NACE CP 4—Cathodic Protection Nickel alloys, 376–377
Specialist, 7 Nickel anodic reaction, 38
NACE International Corrosion Nickel-chrome, 632
Network, 11 Nickel-free environment-friendly
NACE Marine Coating Inspector seals, 142
Course, 7 Nionel, 378
NACE Protective Coatings and Nitrates:
Linings, 7 in fresh water, 272
Nalgene, 382 in soils, 405
NASA Kennedy Space Center (KSC), Nitric acids:
353, 359 and gold coatings, 474
Nascent hydrogen, 397 and sulfuric acids, 212
National Association of Corrosion Nitridation, 626, 705
Engineers (NACE) International: Nitrogen oxides (NO ):
x
Basic Corrosion Course, 7 in industrial atmospheres, 330
on blasting, 658 as pollutant, 340