Page 265 - Materials Science and Engineering An Introduction
P. 265

7.12 Recrystallization  •  237

              Figure 7.21
              Photomicrographs
              showing several stages of
              the recrystallization and
              grain growth of brass.
              (a) Cold-worked
              (33%CW) grain struc-
              ture. (b) Initial stage of
              recrystallization after
              heating for 3 s at 580 C
              (1075 F); the very small
              grains are those that
              have recrystallized.
              (c) Partial replacement
              of cold-worked grains by
              recrystallized ones (4 s
              at 580 C). (d) Complete
              recrystallization (8 s at         (a)                                   (b)
              580 C). (e) Grain growth                        100  m                               100  m
              after 15 min at 580 C.
              (f) Grain growth after
              10 min at 700 C (1290 F).
              All photomicrographs
              70 .
              (Photomicrographs courtesy
              of J. E. Burke, General
              Electric Company.)













                                                  (c)                                  (d)
                                                               100  m                              100  m






















                                                  (e)                                  (f)
                                                               100  m                              100  m
   260   261   262   263   264   265   266   267   268   269   270