Page 113 - Mechanics of Asphalt Microstructure and Micromechanics
P. 113

Experimental Methods to Characterize the Heterogeneous Strain F ield   105


                 Step 3: The particles were ranked by similarity index in ascending order and the top
              two were assigned a closeness value of 1.
                 Step 4: The previous two steps were repeated for different particle characteristics
              and the closeness values for each of the five particles was summed. The particle with
              the largest closeness value was identified as the matching particle.




























































              FIGURE 4.6  Numbering in undeformed and deformed confi guration (Image 10).
   108   109   110   111   112   113   114   115   116   117   118