Section 4.0 - Slags                                          311







































                              Figure 14. Relationship between the area of the devitrification peak and slag content.



                              Table 6. Hydration Rate of Cement Compounds Containing Slag

                                Compound                            Stages
                                                        I             II             III

                                C A                 Retardation   Retardation   Acceleration
                                 3
                                Alite              Retardation*  Retardation*   Acceleration

                                C S                 Retardation   Retardation   Acceleration
                                 3
                                 C A + CaSO         Retardation   Retardation   Acceleration
                                 3         4
                                C A + CaSO +
                                           4
                                 3
                                   Ca(OH) 2        Acceleration   Acceleration  Acceleration
                                     * Under certain conditions, alite may be accelerated when high surface
                                     area slag is used.