350    CHAPTER 13 A concise filtergram wear particle atlas

















                                                 200mm                               100mm
                          (a)                               (b)
                         FIGURE 13.64
                         The varnish deposit and the damages on the gearbox bearing pads: (a) the varnish deposit
                         and the onset damage on bearing #3; (b) the moderate damage in the edge of bearing #5 due
                         to the varnish deposit.















                          (a)                     100 µm      (b)                50mm
                         FIGURE 13.65
                         The damaged rubber seal generated significant amount of rubber particles: (a) a typical
                         rubber particles on filtergram (200 ); (b) the damaged rubber seal clogged in the inlet of
                         bearing #5.













                          (a)                  50µm         (b)                  100µm
                         FIGURE 13.66
                         The microorganism from a new oil sample (200 ): (a) a microorganism; (b) a microorganism.