Page 442 - Handbook of Materials Failure Analysis
P. 442

440    CHAPTER 16 Degradation of protective PVD coatings




                         [111] Oka YI, Yoshida T, Yamada Y, Yasui T, Hata S. Evaluation of erosion and fatigue resis-
                              tance of ion plated chromium nitride applied to turbine blades. Wear 2007;263:379–85.
                         [112] Puchi-Cabrera ES, Staia MH, Lesage J, Gil L, Villalobos-Gutierrez C, La Barbera-
                              Sosa J, et al. Fatigue behavior of AA7075-T6 aluminum alloy coated with ZrN by
                              PVD. Int J Fatigue 2008;30:1220–30.
                         [113] Gelfi M, La Vecchia GM, Lecis N, Troglio S. Relationship between through-thickness
                              residual stress of CrN-PVD coatings and fatigue nucleation sites. Surf Coat Technol
                              2005;192:263–8.
                         [114] Gerdes C, Karimi A, Bieler HW. Water droplet erosion and microstructure of laser
                              nitride Ti-6Al-4V. Wear 1995;186–187:368–74.
                         [115] Godoy C, Mancosu RD, Lima MM, Brandao D, Housden J, Avelar-Batista JC. Influ-
                              ence of plasma nitriding and PAPVD Cr 1-x N x coating on the cavitation erosion resis-
                              tance of an AISI 1045 steel. Surf Coat Technol 2006;200:5370–8.
                         [116] Han S, Lin JH, Kuo JJ, He JL, Shih HC. The cavitation-erosion phenomenon of chro-
                              mium nitride coatings deposited using cathodic arc plasma deposition on steel. Surf
                              Coat Technol 2002;161:20–5.
                         [117] Iwai Y, Honda T, Yamada H, Matsubara T, Larsson M, Hogmark S. Evaluation of wear
                              resistance of thin hard coatings by a new solid particle impact test. Wear
                              2001;251:861–7.
                         [118] Iwai Y, Miyajima T, Honda T, Matsubara T, Kanda K, Hogmark S. Evaluation of ero-
                              sive wear resistance of TiN coatings by a slurry jet impact test. Wear 2006;261:112–8.
                         [119] Mann BS, Arya V, Maiti AK, Rao MUB, Joshi P. Corrosion and erosion performance of
                              HVOF/TiAlN PVD coatings and candidate materials for high pressure gate valve appli-
                              cation. Wear 2006;260:75–82.
                         [120] Krella A, Czyz ˙niewski A. Cavitation erosion resistance of nanocrystalline TiN coating
                              deposited on stainless steel. Wear 2008;265:963–70.
                         [121] Munsterer S, Kohlhof K. Cavitation protection by low temperature TiCN coatings. Surf
                              Coat Technol 1995;74–75:642–7.
                         [122] Krella A. An experimental parameter of cavitation erosion resistance for TiN coatings.
                              Wear 2011;270:252–7.
                         [123] Gachon Y, Ienny P, Forner A, Farges G, Sainte Catherine MC, Vannes AB. Erosion by
                              solid particles ofW/W–N multilayer coatings obtained by PVD process. Surf Coat
                              Technol 1999;113:140–8.
   437   438   439   440   441   442   443   444   445   446   447