Page 50 - Carbon Nanotube Fibres and Yarns
P. 50
Carbon nanotube fibers spun directly from furnace 43
(A) (B)
(C) (D)
Fig. 3.3 TEM images of CNTs synthesized at different temperatures: (A) 1200°C, (B)
1300°C, (C) 1400°C, and (D) 1500°C. (Reproduced with permission from Hou G, Chauhan D,
Ng V, Xu C, Yin Z, Paine M, et al. Gas phase pyrolysis synthesis of carbon nanotubes at high
temperature. Mater. Des. 132 (2017) 112–118.)
Fig. 3.4 Raman RBM peaks of CNTs at different synthesis temperature: (A) 514 nm laser,
and (B) 785 nm laser. (Reproduced with permission from Hou G, Chauhan D, Ng V, Xu C, Yin
Z, Paine M, et al. Gas phase pyrolysis synthesis of carbon nanotubes at high temperature.
Mater. Des. 132 (2017) 112–118.)