Page 379 - Challenges in Corrosion Costs Causes Consequences and Control(2015)
P. 379

CORROSION DAMAGE, DEFECTS, AND FAILURES                         357











                  1 .0 in.
                 25.4 mm




                                            (a)






                            1–1/4Cr 1/2Mo    309 weld overlay


                             400 μm




















                                            (b)

                                        1
                                            1
            Figure 5.39 309 uniform overlay on 1 / 4 Cr / 2 Mo boiler tube after service in coal-fired boiler.
            (a) Weld overlay with visible weld beads. (b) Weld overlay cross section showing no corrosion
            and no cracking. (Figure originally published in Reference 29. Reproduced with permission of
            the Canadian Institute of Mining, Metallurgy and Petroleum. www.cim.org.)