Page 187 - Handbook of Plastics Technologies
P. 187

THERMOSETS


                                                          THERMOSETS                         3.57


                                            TABLE 3.55  Phenylethynyl Cross-Linked Polyimide
                                            Composite Properties
                                             Shear strength, psi, room temperature  5,700
                                               177°C                          4,400
                                               48 hr in hydraulic fluid        5,410
                                             Flexural modulus, psi, room temperature  23,000,000
                                               177°C                      22,000,000
                                             Flexural strength, room temperature  268,000
                                               177°C                        190,000







                                                                FIGURE  3.55 Benzocyclobutene-terminated
                                                                polyimide oligomers.






























                                       FIGURE 3.56 Benzocyclobutene cross-linking cure reactions.




                                                              FIGURE  3.57 Benzocyclobutene-terminated
                                                              diketone.