Page 119 - Trenchless Technology Piping Installation and Inspection
P. 119

Existing Pipeline Renewal and Replacement Methods        85

                  3.1.6   The owner authorizes the use of proven materials
                       that serve to enhance the pipe performance specified
                       herein. Proven materials have passed independent
                       laboratory testing, not excluding long-term (10,000
                       hours) structural behavior testing, and have been
                       successfully installed to repair failing existing pipes
                       in the United States for at least 4 years.
                           Documentation for products and installers seeking
                       preapproved status must be submitted no less than
                       2 weeks prior to proposal due date to allow time for
                       adequate consideration. The owner will advise of
                       acceptance or rejection a minimum of three days prior
                       to the due date. All required submittals must be satis-
                       factory to the owner.
           4.  Materials
               4.1   Tube—The sewn tube shall consist of one or more layers of
                  absorbent nonwoven felt fabric and meet the requirements
                  of ASTM F1216-09, Sec. 5.1 or ASTM F1743-08, Sec. 5.2.1 or
                  ASTM D 5813-04, Secs. 5 and 6. The tube shall be con-
                  structed to withstand installation pressures, have sufficient
                  strength to bridge missing pipe, and stretch to fit irregular
                  pipe sections.
                  4.1.1   The wet out tube shall have a relatively uniform
                       thickness that when compressed at installation pres-
                       sures will equal or exceed the calculated minimum
                       design CIPP wall thickness.
                  4.1.2   The tube shall be manufactured to a size that when
                       installed will tightly fit the internal circumference and
                       length of the original pipe. Allowance should be made
                       for circumferential stretching during installation.
                  4.1.3   The outside layer of the tube shall be coated with an
                       impermeable, flexible membrane that will contain
                       the resin and allow the resin impregnation (wet out)
                       procedure to be monitored.
                  4.1.4   The tube shall contain no intermediate or encapsu-
                       lated elastomeric layers. No material shall be
                       included in the tube that may cause delamination in
                       the cured CIPP. No dry or unsaturated layers shall be
                       evident.
                  4.1.5   The wall color of the interior pipe surface of CIPP
                       after installation shall be a relatively light reflective
                       color so that a clear detailed examination with closed
                       circuit television inspection equipment may be
                       made.
                  4.1.6   Seams in the tube shall be stronger than the non-
                       seamed felt material.