494                        G. SHATIL AND h? ERSOY



























                                 2      3      4      5      6      7
                                            log(experimenta1 life)

























                                 2      3      4      5      6       7
                                            log(experimenta1 life)

             Fig. 6. Life prediction of the rhombic plate specimens using a subsurface shear strain damage
             analysis and two different strain paths, where the damage summations are carried out up to: (a)
             p = lmm; and (b)p = 0.5mm.