Fig.  4.  (a) Crack initiation  points marked  by  arrow head  in optical micrograph; (b) SEM fractograph taken from area
          marked as 'X' in Fig. 4(a); (c) SEM fractograph from area marked as 'Y in Fig. 4(a). Arrows indicate crack growth directions
          (dark line at the centre indicates the cut-mark along which fracture surface was cut into two pieces for SEM observation).